Abstract:
bnormal colour wag observed OH the surface of forged LF6 after being anodized with sulphurie acid,which effects quality and performance of the material.To determine the reason for tllis abnormal colour,a series of tests were designed and conducted.Tests results show that the main reasons of the abnormal colour are the metal elements of the alloy and the long period of processing.