|Table of Contents|

Study on erosion wear properties and its mechanism of C/SiC composite nozzle(PDF)

《火箭推进》[ISSN:1672-9374/CN:CN 61-1436/V]

Issue:
2019年01期
Page:
53-58
Research Field:
研究与设计
Publishing date:

Info

Title:
Study on erosion wear properties and its mechanism of C/SiC composite nozzle
Author(s):
YANG XiaohuiCAO PeiWANG YiBAI Longteng
(Xi'an Aerospace Propulsion Institute, Xi'an 710100, China)
Keywords:
C/SiC composites nozzle erosion wear microstructure erosion mechanism
PACS:
V250.1
DOI:
-
Abstract:
For validating application feasibility of C/SiC composite nozzle in the liquid-solid two phase flow in the actual environment, the C/SiC composite nozzle was fabricated by the chemical vapor deposition process and preceramic polymer impregnation pyrolysis process, combined with engineering application background of C/SiC composites nozzle. Long life assessment was also carried out in actual enviroment. Based on erosion wear characteristics of the C/SiC composites nozzles during the assessment process, SEM analysis was made used for the liquid-solid two-phase flow characteristic, microstructure evolution and the erosion wear mechanisms with different location of the nozzle. The results show that the C/SiC composite nozzle exhibits an increasing degree of erosion wear from the inlet end to the outlet section of the test piece. The erosion wear mode is mainly composed of erosion pit and thermal stress “crash”, and the main cause of the “biasing” phenomenon is the anisotropy of the C/SiC composite and the non-uniformity of the liquid-two-phase flow.

References:

[1] 徐永东,张立同,成来飞,等.三维针刺碳/碳化硅陶瓷基复合材料及其摩擦磨损性能[J].航空材料学报,2007,27(1):28-32.
[2] 徐兴亚,张立同,成来飞,等.碳陶刹车材料的研究进展[J].航空制造技术,2014(6):100-103.
[3] 徐永东,张立同,成来飞,等.碳/碳化硅摩阻复合材料的研究进展[J].硅酸盐学报,2006,34(8):992-999.
[4] 白龙腾,杨晓辉,王毅,等.低成本制造C/SiC复合材料的热物理性能研究[J].火箭推进,2016,42(1):58-65.
BAI L T,YANG X H,WANG Y,et al.Research on thermal physical properties of C/SiC composite manufactured with low-cost process[J].Journal of Rocket Propulsion,2016, 42(1): 58-65.
[5] KRENKEL W.Design of ceramic brake pads and disks[J].Ceram Eng Sci Proc, 2002, 23(3): 319-330.
[6] VAIDYARAMAN S, PURDY M, WALKER T, et al.C/SiC material evaluation for aircraft brake applications[C]//Proceedings of 4th International Conference on High Temperature Ceramic Matrix Composites.Munich,Germany:[s.n.], 2001: 802-808.
[7] KRENKEL W.C/C-SiC composites for hot structures and advanced friction systems[J].Ceram Eng Sci Proc, 2003, 24(4): 592.
[8] 康进兴,赵文轸,朱金华.材料抗冲蚀性的研究进展[J].材料保护,2001,34(10):22-23.
[9] 马颖,任峻,李元东,等.冲蚀磨损研究的进展[J].兰州理工大学学报,2005,31(1):21-25.
[10] 陈茜,鲍崇高.液/固两相流冲蚀磨损机理及材料应用现状[J].铸造技术,2005,26(6):548-550.
[11] 马颖,任峻,李元东,等.冲蚀磨损研究的进展[J].兰州理工大学学报,2005,31(1):21-25.

Memo

Memo:
-
Last Update: 2019-02-20