PDF下载 分享
[1]王 毅,李洪春,郭春峰.沉积温度对CVD-SiC涂层显微结构的影响[J].火箭推进,2014,40(04):50-56.
 WANG Yi,LI Hong-chun,GUO Chun-feng.Effect of deposition temperature on microstructure of SiC coating prepared by CVD process[J].Journal of Rocket Propulsion,2014,40(04):50-56.
点击复制

沉积温度对CVD-SiC涂层显微结构的影响

参考文献/References:

[1]张立同, 成来飞. 连续纤维增韧陶瓷基复合材料可持续发展战略探讨[J]. 复合材料学报, 2007, 24(2): 1-6.
[2]NASLAIN R, CHRISTIN F. SiC-matrix composite ma- terials for advanced jet engines [J]. MRS Bull, 2003, 28(9): 654-658.
[3]NASLAIN R. Design, preparation and properties of non- oxide CMCs for application in engines and nuclear reactors: an overview[J]. Composites Science and Tech- nology, 2004, 64(2): 155-170.
[4]闫联生, 邹武. 沉积温度对碳化硅基体及其复合材料的影响[J]. 固体火箭技术, 1999, 22(1): 68-71.
[5]张长瑞, 刘荣军,曹英斌. 沉积温度对 CVD SiC 涂层显微结构的影响[J]. 无机材料学报, 2007, 22(1): 153-158.
[6]KIM H, CHUNG G Y, KOO H H, et al. Effects of process parameters for the preparation of C/SiC composites in the F-Chemical vapor infiltration reactor[J]. Korean Journal of Chemical Engineering, 2004, 21(5): 929-934.
[7]朱庆山, 邱学良. 化学气相沉积制备 SiC 涂层-Ⅱ. 动力学研究[J]. 化工冶金, 1998, 19(4): 289-292.
[8]XU Y, CHENG L, ZHANG L. Carbon/silicon carbide composites prepared by chemical vapor infiltration combined with silicon melt infiltration[J]. Carbon, 1999, 37(8): 1179-1187.
[9]XU Y, CHENG L, ZHANG L. Composition, micro- structure, and thermal stability of silicon carbide chemical vapor deposited at low temperatures[J]. Journal of Materials Processing Technology, 2000, 101(1/3): 47-51.
[10]LANGLAIS F, LOUMAGNE F, LESPIAUX D, et al. Kinetic processes in the CVD of SiC from CH3SiCl3-H2 in a vertical hot-wall reactor[J]. Journal de Physique Iv, 1995, 5: 105-112.
[11]卢翠英, 成来飞, 赵春年, 等. 温度对化学气相沉积碳化硅涂层的影响[J]. 材料科学与工艺, 2010, 18(4): 575- 578.
[12]徐永东, 张立同. 常压化学气相沉积 SiC 的组织结构及其稳定性[J]. 航空学报, 1997, 18(1): 123-126.
[13]朱庆山, 邱学良. 化学气相沉积制备 SiC 涂层Ⅰ. 热力学研究[J]. 化工冶金, 1998, 19(3): 193-198.
[14]BESMANN T, STINTON D, MATLIN W. Chemical vapor infiltration process modeling and optimization[R]. Oak Ridge, USA: Oak Ridge National Lab, 1995.
[15]NASLAIN R., LANGLAIS F, FEDOU R. The CVI- processing of ceramic matrix composites[J]. Journal de Physique Colloques, 1989, 50(C5): 191-207.
[16]LOUMAGNE F, LANGLAIS F, NASLAIN R. Kinetic laws of the chemical process in the CVD of SiC ceramics from CH3SiCl3-H2 precursor[J]. Journal de Physique IV, 1993, 3: 527-533.
[17]LOUMAGNE F, LANGLAIS F, NASLAIN R. Experi- mental kinetic study of the chemical vapour deposition of SiC-based ceramics from CH3SiCl3/H2 gas precursor [J]. Journal of Crystal Growth 1995, 155(3/4): 198-204.
[18]姚连增. 晶体生长基础[M]. 合肥: 中国科学技术大学出版社, 1995.
[19]刘荣军, 张长瑞, 周新贵, 等. CVD SiC 致密表面涂层制备及表征[J]. 材料工程, 2005 (004): 3-6.
[20]赵松, 史景利, 魏兴海, 等. 沉积温度对碳芯 SiC 纤维微观结构的影响[J]. 宇航材料工艺, 2011, 41(4): 36-40.

备注/Memo

收稿日期:2014-01-21;修回日期:2014-03-26 作者简介:王毅(1981—),男,博士,研究领域为陶瓷基复合材料制备技术

更新日期/Last Update: 1900-01-01