航天推进技术研究院主办
ZHAO Yali,HUI Pu,CUI Shanshan.Analysis of forming defects and improvement of forming technology for a certain type nozzle inner wall[J].Journal of Rocket Propulsion,2019,45(04):63-68.
某型号喷管内壁成形缺陷分析及工艺改进
- Title:
- Analysis of forming defects and improvement of forming technology for a certain type nozzle inner wall
- 文章编号:
- 1672-9374(2019)04-0063-06
- Keywords:
- curved generatrix; wrinkling defect; finite element simulation; improvement of die surface
- 分类号:
- V463
- 文献标志码:
- A
- 摘要:
- 某型号喷管内壁为曲母线回转体零件,采用锥形坯料液压成形的工艺方法加工。成形后零件存在大端周圈起皱及小端喉部下方周向环状突起的缺陷,严重影响产品质量。为提高零件型面及尺寸精度,应用PAM-STAMP钣金数值模拟软件对零件的成形过程进行仿真,观察零件成形过程中坯料在模具型腔内的变形过程,并获得了坯料变形过程中的应力应变分布状况。同时,结合材料塑性成形理论分析,找到了该零件成形缺陷产生的原因,即模具型面及间隙设计不合理。进而,根据分析得出的零件变形规律及应力应变分布状况对模具型面进行设计改进,生产出了满足设计图纸要求的零件。数值模拟得到的零件壁厚及型面间隙与实际零件一致。可见,准确掌握零件变形规律,合理设计模具型面及间隙,消除了零件成形缺陷。
- Abstract:
- The inner wall of a certain nozzle is the revolving parts with curved generatrix,which is hydraulic formed by conical blank.After forming,the part has the defects of wrinkling in the large end and annular protrusion below throat of small end,which seriously affects the quality of products.In order to improve the accuracy of part surface and dimension,PAM-STAMP sheet metal numerical simulation software was used to simulate the forming process of parts,through which the deformation process of blank in the die cavity during the forming process was observed,and the stress and strain distribution during the deformation process of blank was obtained.At the same time,combined with the theory of material plastic forming,the causes of forming defects of the part were found,that is,the design of die surface and clearance was unreasonable.Then,according to the deformation law and stress-strain distribution of the part obtained from the analysis,the design of the die surface was improved,and the part meeting the requirements of the design drawings was produced.The wall thickness and surface clearance obtained by numerical simulation are consistent with the actual parts.It is thus clear that,the forming defects of part can be eliminated by accurately grasping the deformation law of part and reasonably designing the die surface and clearance.
参考文献/References:
[1] 李硕本.冲压工艺学[M].北京:北京机械工业出版社,1982.
[2] 盖玢玢.轴对称拉深成形应变分布规律及圆锥形件起皱破裂研究[D].秦皇岛:燕山大学,2015.
[3] 赵跃俊.基于钣金工艺优化的钣金件结构设计[J].自动化应用,2017(3):46.
[4] 安爱民,陈玉全,汪欢,等.LS-DYNA在汽车冲压件成形过程中的应用研究[J].哈尔滨理工大学学报,2007,12(5):19-22.
[5] 李青义.基于三维模型的钣金零件检验特征提取与识别研究[D].沈阳:沈阳理工大学,2014.
[6] 雒亚涛,张华,郭广西.计算机仿真椭圆钣金件拉深成形技术研究[J].火箭推进,2012,38(6):46-51.LUO Y T,ZHANG H,GUO G X.Computer simulation based deep drawing forming technology for elliptic sheet-metal parts[J].Journal of Rocket Propulsion,2012,38(6):46-51.
[7] 彭必友,傅建,肖兵,等.冲压回弹仿真结果的工艺知识发现技术研究[J].锻压技术,2009,34(3):33-36.
[8] 王远钟,董定福,俞芙芳.数值模拟波动压边力对拉深件成形质量的影响[J].塑性工程学报,2005,12(3):46-50.
[9] 茅杰,马春华,钱宏辉,等.钣金展开计算方法研究及应用[J].制造业自动化,2016,38(10):70-73.
[10] 雒亚涛,王相勇.钛合金弧板类零件冲压成型回弹仿真计算[J].火箭推进,2014,40(2):72-76.LUO Y T,WANG X Y.Simulating calculation for spring-back magnitude of titanium alloy plates with arc formed by stamping[J].Journal of Rocket Propulsion,2014,40(2):72-76.
[11] 吴勇国,李尚健,李志刚.板料成形有限元分析的显式算法[J].塑性工程学报,1995,2(3):31-36.
[12] 李泷杲.金属板料成形有限元模拟基础:PAMSTAMP2G(Autostamp)[M].北京:北京航空航天大学出版社,2008.
[13] 李尚健.金属塑性成形过程模拟[M].北京:机械工业出版社,1999.
[14] 刘红升.板料成形仿真的起皱预测算法研究[D].淄博:山东理工大学,2013.
[15] 郝军伟.基于Autoform右背门里板拉伸起皱问题的调试处理[J].模具制造,2017,17(5):1-7.
[16] 张锦龙.钣金加工工艺研究[J].现代制造技术与装备,2017(2):136-137.
备注/Memo
收稿日期:2018-08-15; 修回日期:2018-12-20基金项目:中国航天科技集团重大工艺专项资助项目(ZDGY2013-22)作者简介:赵雅丽(1982—),女,硕士,研究领域为材料塑性成形