WANG Fuyuan,YANG Xiaohui,WANG Yi,et al.Effect of water vapor and oxygen corrosion environment on thermal diffusivity of 2D C/SiC composites[J].Journal of Rocket Propulsion,2017,43(04):23-28.
水氧腐蚀环境对2D CSiC热扩散性能的作用机制研究
- Title:
- Effect of water vapor and oxygen corrosion environment on thermal diffusivity of 2D C/SiC composites
- 分类号:
- V250.3-34
- 文献标志码:
- A
- 摘要:
- 通过对不同温度条件下,水氧腐蚀前后2D C/SiC复合材料热扩散性能的演变规律,研究了环境损伤对C/SiC复合材料热扩散性能的作用机制。在水蒸气和氧气混合环境下,C/SiC复合材料内部气孔率增加,同时在材料表面有氧化物形成。材料内部出现的气孔,阻断了热流在材料内部的传输,使得热扩散性能呈现出直线下降的趋势。氧化物的形成,在一定程度上封填裂纹,有助于热量的传输,能够在一定程度上改善材料热扩散性能。
- Abstract:
- The effect of environmental corrosion on thermal diffusivity of 2D C/SiC composites is investigated by the microstructural evolution of water vapor and oxygen corrosion under the conditions of different temperatures. In the water vapor and oxygen mixture environment, the porosity increases and the oxide forms in the composites. The pores inside the composites interrupts the heat flow transmission, which results in almost linear reduction of thermal diffusivity of composites. The oxide forming at high corrosion temperature fills up the matrix cracks, which is conducive to thermal transmission and can improve the thermal diffusivity in the composites.
参考文献/References:
[1]张立同, 成来飞. 连续纤维增韧陶瓷基复合材料可持续发展战略探讨[J]. 复合材料学报, 2007, 24(2): 1-6.
[2]CHENG L, XU Y, ZHANG L, et al. Corrosion of a 3D-C/SiC composite in salt vapor environments [J]. Carbon, 2002, 40(1): 877-82.
[3]葛明和, 姚世强,安鹏. 200N Cf/SiC复合材料推力器研制[J]. 火箭推进, 2016, 42(3): 15-20.
GE Minghe, YAO Shiqiang, AN Peng. Development of 200N thruster made from Cf/SiC composite[J]. Journal of rocket propulsion, 2016, 42(3): 15-20.
[4]LI S, FENG Z, LIU Y, YANG W, et al. Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures[J]. Corros science, 2010 (52): 2837-45.
[5]白龙腾, 杨晓辉, 王毅, 等. 低成本制造C/SiC复合材料的热物理性能研究[J]. 火箭推进, 2016, 42(1): 58-65.
BAI Longteng, YANG Xiaohui, WANG Yi, et al. Research on thermal physical properties of C/SiC composite manufactured with low-cost process[J]. Journal of rocket propulsion, 2016, 42(1): 58-65.
[6]CHENG L, XU Y, ZHANG Q, et al. Thermal diffusivity of 3D C/SiC composites from room temperature to 1400℃ [J]. Carbon, 2003, 41(1): 7-11.
[7]邹林华, 黄伯云, 黄启中, 等. C/C 复合材料的导热系数[J]. 中国有色金属学报, 1997, 7(4): 132-134
[8]MCDONALD K R, DRYDEN J R, ZOK F W. Effects of matrix cracks on the thermal diffusivity of a fiber- reinforced ceramic composite[J]. Journal of am ceram soc, 2001 (84): 2015-2021.
[9]殷小玮. 3D C/SiC复合材料的环境氧化行为[D]. 西安: 西北工业大学, 2001.
[10]魏玺. 3D C/SiC复合材料氧化机理分析及氧化动力学模型[D]. 西安: 西北工业大学, 2004.
备注/Memo
收稿日期:2017-02-18;修回日期:2017-03-15 作者简介:王芙愿(1986—),男,博士,研究领域为陶瓷基复合材料及高温结构材料