- 摘要:
- 为验证C/SiC复合材料喷嘴在液-固两相流实际环境中的应用可行性,采用化学气相沉积工艺和先驱体浸渍-裂解工艺制备了C/SiC复合材料喷嘴的,并充分结合工程化应用背景需求,对C/SiC复合材料喷嘴在实际应用环境中进行长寿命考核。基于C/SiC复合材料喷嘴在实际应用考核过程中表现出的冲蚀磨损特征,采用SEM手段分析了C/SiC复合材料喷嘴不同位置在液-固两相流中微观结构演变特点,并对其冲蚀磨损机理进行探讨。结果表明:C/SiC复合材料喷嘴从试验件入口段到出口段表现出逐渐加剧的冲蚀磨损程度,冲蚀磨损方式主要由冲蚀凹坑和热应力“崩块”组成,而“偏磨”现象产生的主要原因为C/SiC复合材料各向异性和液-固两相流的不均匀性所致。
- Abstract:
- For validating application feasibility of C/SiC composite nozzle in the liquid-solid two phase flow in the actual environment, the C/SiC composite nozzle was fabricated by the chemical vapor deposition process and preceramic polymer impregnation pyrolysis process, combined with engineering application background of C/SiC composites nozzle. Long life assessment was also carried out in actual enviroment. Based on erosion wear characteristics of the C/SiC composites nozzles during the assessment process, SEM analysis was made used for the liquid-solid two-phase flow characteristic, microstructure evolution and the erosion wear mechanisms with different location of the nozzle. The results show that the C/SiC composite nozzle exhibits an increasing degree of erosion wear from the inlet end to the outlet section of the test piece. The erosion wear mode is mainly composed of erosion pit and thermal stress “crash”, and the main cause of the “biasing” phenomenon is the anisotropy of the C/SiC composite and the non-uniformity of the liquid-two-phase flow.
参考文献/References:
[1] 徐永东,张立同,成来飞,等.三维针刺碳/碳化硅陶瓷基复合材料及其摩擦磨损性能[J].航空材料学报,2007,27(1):28-32.
[2] 徐兴亚,张立同,成来飞,等.碳陶刹车材料的研究进展[J].航空制造技术,2014(6):100-103.
[3] 徐永东,张立同,成来飞,等.碳/碳化硅摩阻复合材料的研究进展[J].硅酸盐学报,2006,34(8):992-999.
[4] 白龙腾,杨晓辉,王毅,等.低成本制造C/SiC复合材料的热物理性能研究[J].火箭推进,2016,42(1):58-65.
BAI L T,YANG X H,WANG Y,et al.Research on thermal physical properties of C/SiC composite manufactured with low-cost process[J].Journal of Rocket Propulsion,2016, 42(1): 58-65.
[5] KRENKEL W.Design of ceramic brake pads and disks[J].Ceram Eng Sci Proc, 2002, 23(3): 319-330.
[6] VAIDYARAMAN S, PURDY M, WALKER T, et al.C/SiC material evaluation for aircraft brake applications[C]//Proceedings of 4th International Conference on High Temperature Ceramic Matrix Composites.Munich,Germany:[s.n.], 2001: 802-808.
[7] KRENKEL W.C/C-SiC composites for hot structures and advanced friction systems[J].Ceram Eng Sci Proc, 2003, 24(4): 592.
[8] 康进兴,赵文轸,朱金华.材料抗冲蚀性的研究进展[J].材料保护,2001,34(10):22-23.
[9] 马颖,任峻,李元东,等.冲蚀磨损研究的进展[J].兰州理工大学学报,2005,31(1):21-25.
[10] 陈茜,鲍崇高.液/固两相流冲蚀磨损机理及材料应用现状[J].铸造技术,2005,26(6):548-550.
[11] 马颖,任峻,李元东,等.冲蚀磨损研究的进展[J].兰州理工大学学报,2005,31(1):21-25.
相似文献/References:
[1]杨晓辉,王 毅,白龙腾.CVD-PyC界面层和SiC涂层厚度数学计算模型的建立与验证[J].火箭推进,2014,40(05):69.
YANG Xiao-hui,WANG Yi,BAI Long-teng.Establishment and confirmation of mathematical
computational model of thickness of CVD-PyC
interface and SiC coatings[J].Journal of Rocket Propulsion,2014,40(01):69.
[2]白龙腾,杨晓辉,王毅,等.低成本制造C/SiC复合材料的热物理性能研究[J].火箭推进,2016,42(01):58.
BAI Longteng,YANG Xiaohui,WANG Yi,et al.Research on thermal physical properties of C/SiC composite manufactured with low-cost process[J].Journal of Rocket Propulsion,2016,42(01):58.
[3]王芙愿,王毅,杨晓辉,等.改性先驱体制备C/SiC复合材料性能研究[J].火箭推进,2017,43(03):67.
WANG Fuyuan,WANG Yi,YANG Xiaohui,et al.Properties of C/SiC composites prepared
by modified precursor[J].Journal of Rocket Propulsion,2017,43(01):67.
[4]王芙愿,王毅,杨晓辉,等.C/SiC复合材料在1 700 ℃下氧化机制研究[J].火箭推进,2017,43(06):82.
WANG Fuyuan,WANG Yi,YANG Xiaohui,et al.High-temperature oxidation of C/SiC composites at 1 700 ℃[J].Journal of Rocket Propulsion,2017,43(01):82.
备注/Memo
收稿日期:2017-07-12
基金项目:国家自然科学联合基金(u1737112)
作者简介:杨晓辉(1986—),男,博士,研究领域为超高温结构复合材料体系设计、制备工艺及其性能研究